13. Paint on the enamels with a very small brush and let it dry on top of the kiln for a few minutes.14. Prior to inserting the pendant into the kiln, the kiln temperature should be 1550-degrees F with the bricks glowing orange.
15. Put the pendant in the kiln and fire it for 5-10 minutes depending on the enamel thickness. Take it out and let it cool for a few minutes. Caution: Wear proper protection when inserting the pendant into the kiln.
16. Polish the enameled PMC necklace with silver compound and a cloth.